Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® T KR 4357 G6 - PA6T/6-I-GF30 - BASF

Material Data Center offers the following functions for Ultramid® T KR 4357 G6:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid T datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Glass fibre reinforced, impact modified, partially aromatic polyamide for injection molding. High toughness, stiffness and strength, low water absorption, high melting point (295°C).
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.4 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.0 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 9300 / 9000 MPa ISO 527
Stress at break 165 / - MPa ISO 527
Strain at break 3.5 / - % ISO 527
Tensile creep modulus, 1000h * / 6500 MPa ISO 899-1
Charpy impact strength, +23°C 95 / - kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 17 / - kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 295 / * °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 105 / * °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 240 / * °C ISO 75-1/-2
Vicat softening temperature, B 285 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 22.5 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 65 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
Yellow Card available yes / * - -
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 0.8 / * mm -
Yellow Card available yes / * - -
Oxygen index 24 / * % ISO 4589-1/-2
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 1MHz 4.3 / 4.5 - IEC 62631-2-1
Dissipation factor, 1MHz 300 / 400 E-4 IEC 62631-2-1
Volume resistivity 1E13 / 1E12 Ohm*m IEC 62631-3-1
Surface resistivity * / 1E13 Ohm IEC 62631-3-2
Comparative tracking index - / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 4.5 / * % Sim. to ISO 62
Humidity absorption 0.8 / * % Sim. to ISO 62
Density 1370 / - kg/m³ ISO 1183
Material specific propertiesdry / condUnitTest Standard
ISO Data
Viscosity number 130 / * cm³/g ISO 307, 1157, 1628
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 110 °C -
Pre-drying - Time 8 h -
Processing humidity ≤0.15 % -
Melt temperature 310 - 330 °C -
Mold temperature 80 - 120 °C -
Diagrams
Viscosity-shear rate , Ultramid® T KR 4357 G6, PA6T/6-I-GF30, BASF
Shearstress-shear rate , Ultramid® T KR 4357 G6, PA6T/6-I-GF30, BASF
Stress-strain , Ultramid® T KR 4357 G6 (dry), PA6T/6-I-GF30, BASF
Stress-strain , Ultramid® T KR 4357 G6 (cond.), PA6T/6-I-GF30, BASF
Secant modulus-strain , Ultramid® T KR 4357 G6 (dry), PA6T/6-I-GF30, BASF
Secant modulus-strain , Ultramid® T KR 4357 G6 (cond.), PA6T/6-I-GF30, BASF
Stress-strain (isochronous) 23°C, Ultramid® T KR 4357 G6 (cond.), PA6T/6-I-GF30, BASF
Creep modulus-time 23°C, Ultramid® T KR 4357 G6 (cond.), PA6T/6-I-GF30, BASF
Creep curve 23°C, Ultramid® T KR 4357 G6 (cond.), PA6T/6-I-GF30, BASF
Stress-strain (isochronous) 90°C, Ultramid® T KR 4357 G6 (dry), PA6T/6-I-GF30, BASF
Creep modulus-time 90°C, Ultramid® T KR 4357 G6 (dry), PA6T/6-I-GF30, BASF
Creep curve 90°C, Ultramid® T KR 4357 G6 (dry), PA6T/6-I-GF30, BASF
Stress-strain (isochronous) 120°C, Ultramid® T KR 4357 G6 (dry), PA6T/6-I-GF30, BASF
Creep modulus-time 120°C, Ultramid® T KR 4357 G6 (dry), PA6T/6-I-GF30, BASF
Creep curve 120°C, Ultramid® T KR 4357 G6 (dry), PA6T/6-I-GF30, BASF
Specific volume-temperature (pvT) , Ultramid® T KR 4357 G6, PA6T/6-I-GF30, BASF
Tensile modulus-temperature , Ultramid® T KR 4357 G6 (dry), PA6T/6-I-GF30, BASF
Tensile modulus-temperature , Ultramid® T KR 4357 G6 (cond.), PA6T/6-I-GF30, BASF
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Special Characteristics
High impact or impact modified, Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 110 °C
Pre/Post-processing, Pre-drying, Time: 8 h

PROCESSING
injection molding, Melt temperature, range: 310 - 330 °C
injection molding, Melt temperature, recommended: 320 °C
injection molding, Mold temperature, range: 80 - 120 °C
injection molding, Mold temperature, recommended: 100 °C
injection molding, Dwell time, thermoplastics: 5 min
Application examples
Quick connectors, fuel pipes
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.